The standard outlines several critical requirements for extruded profiles: Alloy Designations : Common alloys covered include (high conductivity), (high strength), and (general structural use). Dimensional Tolerances : It establishes two classes of tolerances: Mechanical Properties
While many websites claim to offer a "free JIS H4100 standard PDF," be extremely cautious. Standards are copyrighted intellectual property. Downloading an illegal copy exposes your company to legal risk, and the file may be outdated or corrupted. jis h4100 standard pdf
For instance, a 6061-T6 extruded bar under JIS H4100 must meet a minimum tensile strength of 265 MPa, compared to 310 MPa for the stronger 7075-T6 alloy.
You can purchase the official PDF from:
The JIS H4100 standard applies to:
By purchasing the official document, you ensure you are using the correct, most up-to-date technical information for your critical projects. Downloading an illegal copy exposes your company to
Materials are categorized into Ordinary class or Special class . Special class designations fulfill restrictive structural assignments requiring tighter perpendicularity and angle profiles. Standard Evolution Timeline
: Offers tracking and purchase options for the latest version. Materials are categorized into Ordinary class or Special